Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 90.6 g/10 min @Load 5.00 kg, Temperature 380 °C |
90.6 g/10 min @Load 11.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |