Polymer Property : Cell Length = 0.500 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Cell Length 0.150 - 0.500 mm
0.00591 - 0.0197 in
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.150 - 0.500 mm
0.00591 - 0.0197 in
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.150 - 0.500 mm
0.00591 - 0.0197 in
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..