Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50.8 - 102 microns | 2.00 - 4.00 mil | |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |
|||
Thickness | 25.4 - 102 microns | 1.00 - 4.00 mil | |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Thickness | 25.4 - 102 microns | 1.00 - 4.00 mil | |
Alcoa KAMA 2500 Prime Clear OPS, Shrink Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ IJ181 Graphic Film 2-mil white, vinyl film; Specifically formulated for use on stainless steel; Pressure-activated adhesive for easy sliding, tacking, snap-up and repositioning; Flexible, conforms to moderate curves, .. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive 2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-19 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-37 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-25 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-33 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-87 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3650-10 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-12 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-14 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8626 ES Clear Graphic Film Film 8626 ES is a 2 mil, clear graphic film with pressure-sensitive adhesive. It is designed for flat, single or multi-layered internally illuminated signs or window graphics, both indoors and outdo.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M 3635-91 Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M 3635-0171 Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ FN180Cv3-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Envision™ IJ3730-50 Translucent Film 2-mil vinyl translucent film; Matte surface finish eliminates glare and provides uniform color in reflected and transmitted light; Pressure sensitive adhesive adheres to rigid and flexible substrate.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-11 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-49 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000LF-23 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-54 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000LF-10 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-20 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | Side 1 |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | Side 2 |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |