Thickness 0.0760 - 0.102 microns
0.00299 - 0.00402 mil
Recommended Dry Film
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Thickness 0.0760 - 0.102 microns
0.00299 - 0.00402 mil
Recommended Dry Film
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..