Polymer Property : Thickness = 0.0110 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.279 microns
0.0110 mil
cured laminate, per ply
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Thickness 0.280 microns
0.0110 mil
3000 rpm
Dow SiLK™ I300 280 Semiconductor Dielectric Resin
SiLK™ I300 280 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 280 is compatibl..