Thickness 0.0381 microns
0.00150 mil
Arlon CuClad 6250 Bonding Film
Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu..
Thickness 0.0381 microns
0.00150 mil
Arlon CuClad 6700 Bonding Film
Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu..