Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.140 microns | 0.00551 mil | 3000 rpm |
Dow SiLK™ I300 140 Semiconductor Dielectric Resin SiLK™ I300 140 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 140 is compatibl.. |