Physical Properties Metric English Comments
Thickness 0.2425 - 0.3425 microns
0.009547 - 0.01348 mil
2000-4000 rpm
Dow SiLK™ I300 280 Semiconductor Dielectric Resin
SiLK™ I300 280 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 280 is compatibl..