Thickness 0.250 microns
0.00984 mil
Ni Coating Thickness
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Thickness 0.250 microns
0.00984 mil
Ni Coating Thickness
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
Thickness 0.250 microns
0.00984 mil
Ni Coating Thickness
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..