Physical Properties Metric English Comments
Thickness 12.2 microns
0.480 mil
Honeywell Capran® Emblem™ 1200 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Thickness 12.2 microns
0.480 mil
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film
Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh..
Thickness 12.2 microns
0.480 mil
Honeywell Capran® Emblem™ 1200MT Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hy..