Polymer Property : Thickness = 1.74 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 44.2 microns
1.74 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester
Thickness 44.2 microns
1.74 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester