Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 533 - 1040 microns | 21.0 - 41.0 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Thickness | 889 - 1040 microns | 35.0 - 41.0 mil | Side 1 |
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |