Physical Properties Metric English Comments
Thickness 15000 - 30000 microns
591 - 1180 mil
according to rating
Microtherm Group Slim&Light Fire Resistant Insulation
Microtherm® Slim&Light is a thin lightweight panel of ultra - high performance microporous thermal insulation. It is a highly efficient barrier to flame and heat. Microtherm® Slim&Light allows..
Thickness 3000 - 30000 microns
118 - 1180 mil
Beijing Evergrow Resources Polyurethane Activated Carbon
Features:good strengthgood flexilitygood durabilityApplications:Air purificationInformation provided by Beijing Evergrow Resources.
Thickness 16000 - 30000 microns
630 - 1180 mil
3M EC-2 Cold Shrink End Caps
3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c..