Polymer Property : Thickness = 1200 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 200 - 1200 microns
7.87 - 47.2 mil
OCTAL DPET™ PET Sheet
Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechan..
Thickness 200 - 1200 microns
7.87 - 47.2 mil
Average value: 404 microns Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..