Physical Properties Metric English Comments
Thickness 2700 - 3300 microns
106 - 130 mil
Standard
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window
Description: Shielded Windows WIN-SHIELD™ EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specif..
Thickness 1780 - 3300 microns
70.0 - 130 mil
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Thickness 1780 - 3300 microns
70.0 - 130 mil
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Thickness 1780 - 3300 microns
70.0 - 130 mil
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Thickness 1780 - 3300 microns
70.0 - 130 mil
Zircar Zirconia ZYF-100 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..