Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 366 microns | 14.4 mil | |
Hexcel® HexForce™ 3582 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 366 microns | 14.4 mil | |
Hexcel® HexForce™ 3734 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |