Physical Properties Metric English Comments
Thickness 404 microns
15.9 mil
Hexcel® HexForce™ 48370 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..
Thickness 404 microns
15.9 mil
Hexcel® HexForce™ GA132 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..