Physical Properties Metric English Comments
Thickness 38100 microns
1500 mil
Unifrax FyreWrap® Cable Insulation
Unifrax's FyreWrap® Cable Insulation is a thin, flexible, insulation wrap designed to provide a fire-protective enclosure around cable trays and conduit. The FyreWrap system ensures electrical cir..
Thickness 38100 microns
1500 mil
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct ASTM E2336 System
Unifrax's FyreWrap ™ 1.5 Duct Insulation is a two-layer flexible enclosure for one- and two-hour rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts. Fy..
Thickness 38100 microns
1500 mil
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct Single-Layer System Insulation
Unifrax's FyreWrap ™ 1.5 Duct Insulation is a single-layer flexible enclosure for 1- and 2-hour fire-rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts...
Thickness 38100 microns
1500 mil
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Ventilation Air Duct (VAD) System
Unifrax's FyreWrap ™ 1.5 Duct Insulation is a single-layer flexible duct wrap enclosure for 1- and 2-hour fire-rated ventilation air ducts (VAD). Typical duct types include smoke control, stairwel..
Thickness 38100 microns
1500 mil
Unifrax FyreWrap® EZ 1.5 Duct Insulation Ventilation Air Duct (VAD) System
Unifrax's FyreWrap® EZ 1.5 Duct Insulation is a new optimized single-layer flexible enclosure for 1- and 2-hour fire-rated ventilation air ducts (VAD). Typical duct types include smoke control, st..