Polymer Property : Thickness = 16.0 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Side 1
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon R34661R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon 51576X015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 356 - 406 microns
14.0 - 16.0 mil
Overall
Arlon 51946C015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..