Polymer Property : Thickness = 183 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 183 microns
7.20 mil
Hexcel® HexForce™ 160 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..
Thickness 183 microns
7.20 mil
Typical; ASTM D374
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Thickness 183 microns
7.20 mil
Total; ASTM D3652
3M 438 Premium Performance Aluminum Foil Tape
Thickest non-reinforced aluminum tape for heat resistance; smooth easy unwind; clean, straight edges with minimal wrinkling. UL 723 Classified.Information provided by 3M
Thickness 183 - 335 microns
7.20 - 13.2 mil
Wet
3M Scotchkote™ EA5WB WB Epoxy Coating
3M Scotchkote WB Epoxy Coating EA5WB is a member of the expanding range of 3M Scotchkote high performance coating. It has been specifically developed for original equipment manufacture, particularly..
Thickness 183 microns
7.20 mil
Total; ASTM D3652
3M 477 Vinyl Tape
3M™ Vinyl Tape 477 is comprised of a conformable, transparent vinyl backing with a versatile rubber adhesive. It is an excellent tape to use where abrasion resistance, transparency, conformability ..
Thickness 183 microns
7.20 mil
Hexcel® HexForce™ 372 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..