Polymer Property : Thickness = 2.99 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 76.0 microns
2.99 mil
PSA Thickness; Visual
Parker Chomerics C-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
Thickness 76.0 microns
2.99 mil
Standard
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness 76.0 microns
2.99 mil
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade
DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib..
Thickness 76.0 microns
2.99 mil
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade
DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip ..
Thickness 76.0 microns
2.99 mil
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re..
Thickness 76.0 microns
2.99 mil
Eastman D4032-F Polyethylene  (discontinued **)
D4032-F is a low density, fractional-melt formulation which contains no slip and medium antiblock. It is designed for film applications requiring exceptional toughness, such as in heavy-duty shippi..