Polymer Property : Thickness = 2063 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon 920-20Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape  (discontinued **)
Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon 920-20Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon 920-20Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon LW202Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon LW202Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon LW202Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 49210 - 52390 microns
1938 - 2063 mil
Width
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape..