Polymer Property : Thickness = 21.6 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 21.6 microns
0.850 mil
Nominal; ExxonMobil Method
ExxonMobil Bicor® 85 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..