Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 612 microns | 24.1 mil | Typical; ASTM D374 |
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |