Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 729 microns | 28.7 mil | Typical; ASTM D374 |
DuPont™ Nomex® 410 Paper, 29 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 730 microns | 28.7 mil | |
Zoltek Pyron® Plain Weave Fabric Oxidized Pan Fiber Oxidized Pan FiberApplications include: Industrial Flame and Thermal Insulation |