Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 86.4 microns | 3.40 mil | Nominal |
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 86.4 microns | 3.40 mil | |
ExxonMobil Label-Lyte® 85 LP-200M Mirror Finish, Metallized, White Opaque OPP for Water-based Patch Label Applications White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. It has an anti-static, "mirror finish" metallized print surface that is coro.. |
|||
Thickness | 86.4 microns | 3.40 mil | Backing; ASTM D3652 |
3M 363L Specialty Foil Tape Linered version of 363Information provided by 3M |
|||
Thickness | 86.4 microns | 3.40 mil | ASTM D3652 |
3M 7300 Masking Film 3M™ 7300 Series Masking Film is a high performance, high temperature wide area masking film that is soft flexing for good drape and conformability.Information provided by 3M |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM010 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM027 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM030 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM037 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM090 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM110 Indoor UL Recognized Brushed Silver Polyester Label Products 3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM120 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM127 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM157 Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FP024900 White Polypropylene Label Products 3M™ White Polypropylene Label Products are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV090 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV1220 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV517 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M PS197 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Thickness | 86.4 microns | 3.40 mil | Facestock |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Thickness | 86.4 microns | 3.40 mil | Facestock |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM057 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FM167 Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV030 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV230 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M PS190 White Yupo™ TIS Label Products 3M™ White Yupo™ TIS Label Products are white treated polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a g.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M PS472 White Yupo™ EDP Label Product 3M™ White Yupo™ EDP Label Products PS470 and PS472 are matte white opaque polypropylene materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesiv.. |
|||
Thickness | 86.4 microns | 3.40 mil | Facestock |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 86.4 microns | 3.40 mil | Facestock |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Thickness | 86.4 microns | 3.40 mil | Liner |
3M FV037 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 86.4 microns | 3.40 mil | Facestock |
3M FV038 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |