Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 600 - 3000 microns | 23.6 - 118 mil | plus or minus 100 microns |
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 600 - 3000 microns | 23.6 - 118 mil | plus or minus 100 microns |
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.6 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 1000 - 3000 microns | 39.4 - 118 mil | Average value: 1100 microns Grade Count:26 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.5 |
Sinotek Materials A Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.7 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |