Polymer Property : Thickness = 32.5 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 32.5 microns
1.28 mil
Cured Ply Thickness
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..