Physical Properties Metric English Comments
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri..
Thickness 762 - 838 microns
30.0 - 33.0 mil
Overall
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon 930-125Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon 30580R030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Side 1
Arlon 30580R030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon 930-10Xxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon LW301Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 686 - 838 microns
27.0 - 33.0 mil
Overall
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..