Physical Properties Metric English Comments
Thickness 34.0 - 45.0 microns
1.34 - 1.77 mil
Fired
Lord Adhesives Metech 7600A Cermet Multilayer Dielectric Composition
Dielectric composition 7600A is a glass-ceramic insulative film designed for use in high density multilayer hybrid circuits using either gold or palladium-silver conductors. 7600A fires at 850°C ..