Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 864 microns | 34.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 864 microns | 34.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 864 microns | 34.0 mil | |
Polystrand ThermoPro™ IE7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |