Thickness 35.0 microns
1.38 mil
± 2.5%; ASTM-252-78
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 35 µm)
PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro..