Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2030 - 9530 microns | 80.0 - 375 mil | Range of Thicknesses Available |
Rogers Corporation Poron® Shock Seal™ 4790-79-12 Urethane Foam, Industrial Grade Thickness: 0.080"- 0.375"Color: BlackInformation provided by Rogers Corporation. |