Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 38.1 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 20.0 - 38.1 microns
0.787 - 1.50 mil
Average value: 27.6 microns Grade Count:12
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Thickness 25.4 - 38.1 microns
1.00 - 1.50 mil
Side 1
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 25.4 - 38.1 microns
1.00 - 1.50 mil
Side 2
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 25.4 - 38.1 microns
1.00 - 1.50 mil
Average value: 32.9 microns Grade Count:11
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Copyright © lookpolymers.com All Rights Reserved