Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 399 microns | 15.7 mil | |
Hexcel® HexForce™ 3783 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 399 microns | 15.7 mil | |