Physical Properties Metric English Comments
Thickness 3000 - 4000 microns
118 - 157 mil
Beijing Evergrow Resources BF-3 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..