Physical Properties Metric English Comments
Thickness 43.4 microns
1.71 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester
Thickness 43.4 microns
1.71 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester