Physical Properties Metric English Comments
Thickness 3050 - 4570 microns
120 - 180 mil
Zircar Zirconia ZYF-150 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..
Thickness 3050 - 4570 microns
120 - 180 mil
Zircar Zirconia ZYF-150 Zirconia Felt Insulation
Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains..