Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 130 microns | 5.10 mil | |
Hexcel® HexForce™ 4522 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 130 microns | 5.10 mil | ASTM D3652 |
3M 101+ Value Masking Tape 3M™ Value Masking Tape 101+ is a tan colored crepe paper masking tape for holding, bundling, sealing, and non-critical masking applications where a pressure sensitive tape is needed.Information pro.. |
|||
Thickness | 130 microns | 5.10 mil | Total; ASTM D3752 |
3M 480 Polyethylene Tape 3M™ Polyethylene Tape 480 has a transparent polyethylene backing with a long aging transparent acrylic adhesive. It can be used for splicing and repairing polyethylene sheeting. It is also recommen.. |