Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | <= 5080 microns | <= 200 mil | Cured film, activator cure |
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are form.. |