Polymer Property : Thickness = 6.30 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 130 - 160 microns
5.12 - 6.30 mil
ASTM-D645
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier
GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv..
Thickness 140 - 160 microns
5.51 - 6.30 mil
ASTM D374
CEN® Electronic Material CV Polyimide Film, 6 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..
Thickness 140 - 160 microns
5.51 - 6.30 mil
CEN® Electronic Material CN Polyimide Film, 6 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..