Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1650 microns | 65.0 mil | Release Liner |
3M 9665 Adhesive Transfer Tape with 3M Adhesive 400 3M™ Adhesive Transfer Tapes 463, 465, 9457 and 9665 with 3M™ Adhesive 400 are ideal for bonding together a wide variety of similar and dissimilar materials such as metals, glass, wood, papers, pai.. |
|||
Thickness | 1650 microns | 65.0 mil | ASTM D4325 |
3M Scotch™ 2228 Rubber Mastic Tape 3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-st.. |