Physical Properties Metric English Comments
Thickness 7.50 microns
0.295 mil
ASTM D374
Chesterton 850 Premium Sealing Tape
Description: Chesterton® 850 Premium Sealing Tape is a high density, moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually ..