Physical Properties Metric English Comments
Thickness 1980 microns
78.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32960X078 0.078" (1.98 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flame Resistant Silicone PuttyAppearance: Gray colored, high viscosity gum on polymer ..
Thickness 1980 microns
78.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 32960X078 0.078" (1.98 mm) Uncured Silicone Rubber on Polyester Film Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flame Resistant Silicone PuttyAppearance: Gray colored, high viscosity gum on polymer ..
Thickness 1980 microns
78.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 32980X078 0.078" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ma..