Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 88.9 microns | 3.50 mil | without adhesive |
3M 1080 Vinyl Film Dual cast vinyl film in an array of colors; Five distinctive-looking finishes-matte, satin, gloss, carbon fiber and brushed metal; Use the film right out-of-the-box without graphic protection; Press.. |
|||
Thickness | 88.9 microns | 3.50 mil | Total |
3M 1125 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 88.9 microns | 3.50 mil | Total |
3M 1126 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 2 |
Arlon 28571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | >= 88.9 microns | >= 3.50 mil | Side 2 |
Arlon 28941C015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 88.9 microns | 3.50 mil | side 1 silicone; Arlon SQA-TMS-003 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Thickness | 88.9 microns | 3.50 mil | Release Liner |
3M ATG 987 Tape 3M™ ATG Adhesive Transfer Tape 987 is a 1.7 mil, 400 acrylic, reverse wound, pressure sensitive adhesive on a densified kraft paper liner. Utility grade tape. For use with Scotch® ATG Adhesive App.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV031 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV090 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV09D Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV1222 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV291 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV292 White Vinyl Label Products 3M™ White Vinyl Label Products FV291 and FV292 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl label products utilize 3M™ Adhesive P14.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV855 Tire Vinyl Label Products 3M™ Tire Vinyl Label Products FV852 and FV855 are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling t.. |
|||
Thickness | 88.9 microns | 3.50 mil | Wet |
3M Scotchkote™ GP 830 WB Epoxy Primer 3M Scotchkote WB Epoxy Primer GP 830 is a member of a range of Scotchkote waterborne coatings and has been specifically developed as a primer/tie coat for use on sealed mineral surfaces and existing.. |
|||
Thickness | 88.9 microns | 3.50 mil | Prime Coated 2113 Fiberglass, Substrate |
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho.. |
|||
Thickness | 88.9 microns | 3.50 mil | Caliper; ASTM D645 |
3M 6141 Light Duty Water Activated Paper Tape 3M™ Light Duty Water Activated Paper Tape 6141 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high-tack, water-activated, modified cornstar.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Thickness | 88.9 microns | 3.50 mil | layer 1; Arlon SQA-TMS-003 |
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV033 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV034 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Total; ASTM D3752 |
3M 5180 General Purpose PTFE Skived Film Tapes 3M™ General Purpose PTFE Skived Film Tapes are film backing with a silicone adhesive.Information provided by 3M |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV024702 White Vinyl Label Products 3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens.. |
|||
Thickness | 88.9 microns | 3.50 mil | Facestock |
3M FV037 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 88.9 microns | 3.50 mil | Liner |
Dielectric Polymers NT-988 High Tack Laminating Adhesive
(discontinued **) Acrylic copolymer adhesive with silicone treated release paper liner.Features: Excellent adhesion to low surface energy substratesCompatible with most printing inksApplications: Mounting a wide vari.. |
|||
Thickness | 88.9 microns | 3.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 48271R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater .. |
|||
Thickness | 88.9 microns | 3.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |