Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 241 microns | 9.49 mil | |
Polystrand ThermoPro™ IE7020 Unitape Unidirectional Polyethylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Thickness | 241 microns | 9.49 mil | |
Polystrand ThermoPro™ IE7021 ECR Unitape Unidirectional Polyethylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |