Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 241 - 292 microns | 9.50 - 11.5 mil | Overall |
Arlon 49581R101 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 241 microns | 9.50 mil | |
Hexcel® HexForce™ 6781 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 241 microns | 9.50 mil | Total; ASTM D3752 |
3M 399FR Flame Retardant Glass Cloth Tape 3M™ Flame Retardant Glass Cloth Tape 399FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typic.. |
|||
Thickness | 241 - 318 microns | 9.50 - 12.5 mil | Side 1 |
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 241 - 292 microns | 9.50 - 11.5 mil | Overall |
Arlon 49581B010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 241 - 292 microns | 9.50 - 11.5 mil | Overall |
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 241 - 292 microns | 9.50 - 11.5 mil | Overall |
Arlon 49583R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 241 microns | 9.50 mil | ASTM D3652 |
3M Scotch® 2525 Performance Flatback Tape Scotch® Performance Flatback Tape 2525 is used in holding, splicing or masking applications where high adhesion strength, high temperature capability and high backing strength are required.Informat.. |
|||
Thickness | 241 - 292 microns | 9.50 - 11.5 mil | Overall |
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 241 microns | 9.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values .. |
|||
Thickness | 241 microns | 9.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values .. |
|||
Thickness | 241 microns | 9.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Thickness | 241 microns | 9.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |