Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 95.0 microns | 3.74 mil | estimated wet film thickness |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Thickness | 95.0 microns | 3.74 mil | estimated wet film thickness |
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,.. |