Physical Properties Metric English Comments
Thickness 2410 microns
95.0 mil
Daikin NEOFLON AF-2400 PFA Film
NEOFLON PFA film is a high performance film made from tetrafluoroethylene and perfluoroalkyl vinyl ether (PFA).Information provided by Daikin Industries.
Thickness 2410 microns
95.0 mil
Daikin NEOFLON NF-2400 FEP Film
NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el..