Polymer Property : Thickness = 97.0 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 2460 microns
97.0 mil
Total Pad; ASTM D3652
3M 5836 Clean-Walk Unframed Mat
3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh..